Question: Copper rod is being reduced from a hot-rolled 3/8-in. diameter to a final diameter of 0.100 in. by wire drawing through a series of dies.

Copper rod is being reduced from a hot-rolled 3/8-in. diameter to a final diameter of 0.100 in. by wire drawing through a series of dies. The final wire should have a yield strength in excess of 50,000 psi and an elongation greater than 10%. Use Figure 17-8 to determine a desirable amount of final cold work. Describe the drawing sequence and the placement of the last intermediate anneal, so that the final product has both the desired size and the desired properties.

Step by Step Solution

3.35 Rating (161 Votes )

There are 3 Steps involved in it

1 Expert Approved Answer
Step: 1 Unlock

The problem deals with the amount of cold work and its effect on material strength and ductility as shown in Figure 178 A quantitative measure of amou... View full answer

blur-text-image
Question Has Been Solved by an Expert!

Get step-by-step solutions from verified subject matter experts

Step: 2 Unlock
Step: 3 Unlock

Document Format (1 attachment)

Word file Icon

916-E-M-S-E-M-S (1417).docx

120 KBs Word File

Students Have Also Explored These Related Materials Science Engineering Questions!