Question: 1 1 4 1 Cold Drawn has a yield point of 9 5 ksiGroup of answer choicesTrueFalse 5 1 6 0 OQT 7 0 0

1141 Cold Drawn has a yield point of 95ksiGroup of answer choicesTrueFalse
5160 OQT 700 has a yield point of 120 ksiGroup of answer choicesTrueFalse
WQT stands for water quenched and temperedGroup of answer choicesTrueFalse
The yield point for 1080 IQT 1100 Steel is 103 ksiGroup of answer choicesTrueFalse
The yield point for 1040 WQT 1300 Steel is 63ksiGroup of answer choicesTrueFalse