Question: 3. Silver is electrodeposted from a flowing solution containing 0.1 M Ag+ and supporting electrolyte Agt + e Ag Calculate the diffusion coefficient if the

3. Silver is electrodeposted from a flowing solution containing 0.1 M Ag+ and supporting electrolyte Agt + e Ag Calculate the diffusion coefficient if the diffusion layer thickness is 0.05 cm and limiting current density is 3.17 mAcm? What is diffusion layer thickness if the limiting current density increases to 160 mAcmat a higher flowing rate? 10