Question: 5 . A rolled Cu - 3 0 wt % Zn plate 0 . 5 0 0 - in . - thick has a 2
A rolled Cu wt Zn plate inthick has a elongation asreceived by thesupplier. The desired specifications for the final sheet are a thickness of inminimum tensile strength of psi, and minimum elongation of Assume that the rolling is conducted so that the width of the sheet is unchanged. Specify all steps in the procedure, including heat treatments.