Question: ( a ) Explain the differences between feature size and resolution in the vector - scan Vat Photopolymerization process. ( b ) Can the layer

(a) Explain the differences between feature size and resolution in the vector-scan Vat Photopolymerization process.
(b) Can the layer thickness be changed in vector-scan VPP? If yes, how?
(c) Why is there a post-curing process in the stereolithography AM? Explain what happens if the postcuring process is not done properly.
(a) Categorize AM feedstock in terms of the physical shape/material state.
(b) Give a material example and an AM process for each category.
(a) Explain the differences between different types of polymers in terms of the molecular bonding mechanisms.
(b) Name an AM process that can be used to fabricate parts from each polymer type.
What are the main differences between chemically induced sintering and liquid-phase sintering? Explain with an example for each process.
(a) A porous bone replacement structure is to be made from stainless steel 316L. Which of the following AM processes would you use for this purpose: PBF or DED? Justify your answer.
(b) If the melting temperature of the alloy feedstock is 1410C, what will be the proper temperature range for solid-state sintering of the part? Show your calculations and explain your response if needed
( a ) Explain the differences between feature

Step by Step Solution

There are 3 Steps involved in it

1 Expert Approved Answer
Step: 1 Unlock blur-text-image
Question Has Been Solved by an Expert!

Get step-by-step solutions from verified subject matter experts

Step: 2 Unlock