The aluminum was deposited in an impure 1.1 g aqueous ammonia aluminum plate. The precipitate was filtered
Fantastic news! We've Found the answer you've been seeking!
Question:
The aluminum was deposited in an impure 1.1 g aqueous ammonia aluminum plate. The precipitate was filtered and ignited at 1000°C to give 0.05 g anhydrous A1,0, calculate% NH AI (SO), in the original organization