Question: Determine the required transformation temperature and micro constituent if eutectoid steel is to have the following hardness values: (a) HRC 38; (b) HRC 42; (c)
(a) HRC 38;
(b) HRC 42;
(c) HRC 48; and
(d) HRC 52.
Step by Step Solution
3.19 Rating (163 Votes )
There are 3 Steps involved in it
a 600 C Pearlit... View full answer