Question: 1 . A linear reciprocating test involved a ball moving back and forth on a flat surface 1 0 , 0 0 0 times. At
A linear reciprocating test involved a ball moving back and forth on a flat surface times. At the end of the test, interferometry was used to measure the wear scar, as shown below. The average crosssectional area of the wear track was found to be mathrm~lm Calculate the wear rate.
Step by Step Solution
There are 3 Steps involved in it
1 Expert Approved Answer
Step: 1 Unlock
Question Has Been Solved by an Expert!
Get step-by-step solutions from verified subject matter experts
Step: 2 Unlock
Step: 3 Unlock