Question: (c) Consider an alloy that is undergoing carburizing process, initially has a uniform carbon concentration of 0.27 wt% and is to be treated at 950C

 (c) Consider an alloy that is undergoing carburizing process, initially has

(c) Consider an alloy that is undergoing carburizing process, initially has a uniform carbon concentration of 0.27 wt% and is to be treated at 950C (1750F). If the concentration of carbon at the surface is suddenly brought to and maintained at 1.32 wt%, how long will it take to achieve a carbon content of 0.85% at a position 0.7 mm below the surface? The diffusion coefficient for carbon in iron at this temperature is 1.6 x 10-11 m2/s; assume that the steel piece is semi-finite