Question: CORROSION ENGINEERING. PLEASE ANSWER ASAP. I WILL LEAVE A GOOD RATING IMMEDIATELY. I PROMISE!! Problem 3 Pitting Corrosion A corrosion pit in SS304 exposed to
CORROSION ENGINEERING. PLEASE ANSWER ASAP. I WILL LEAVE A GOOD RATING IMMEDIATELY. I PROMISE!!

Problem 3 Pitting Corrosion A corrosion pit in SS304 exposed to chloride solution grows to a depth of 2mm in 30 days. The density of the alloy is 7.85g/cm3. SS 304 is composed of approximately 20% Cr,10%Ni,2%Mn,68%Fe. Please assume that the corrosion current density remain constant. a) Please calculate the current density ipit in the inner pit of SS304
Step by Step Solution
There are 3 Steps involved in it
Get step-by-step solutions from verified subject matter experts