Question: Two nominally flat steel surfaces are lapped to give standard deviation of surface heights of 0.15 um and correlation lengths of 1 m. When

Two nominally flat steel surfaces are lapped to give standard deviation of surface heights of 0.15 um and correlation lengths of 1 m. When the surfaces are placed in contact, (a) would you expect the asperity deformation to be elastic, predominately plastic, or elastic- plastic? (b) What is the real area of contact for a normal load of 100 N? Given parameters are composite modulus E* = 110 GPa and H = 8GPa.
Step by Step Solution
There are 3 Steps involved in it
To solve this problem we need to understand surface contact mechanics Lets address both parts of the ... View full answer