Question: The lower yield point for an iron that has an average grain diameter of 5 10 -2 mm is 135MPa (19,500psi). At a grain
The lower yield point for an iron that has an average grain diameter of 5 × 10-2 mm is 135MPa (19,500psi). At a grain diameter of 8 × 10-3 mm, the yield point increases to 260MPa (37,500psi). At what grain diameter will the lower yield point be 205MPa (30,000psi)?
Step by Step Solution
3.51 Rating (181 Votes )
There are 3 Steps involved in it
The best way to solve this problem is to first esta... View full answer
Get step-by-step solutions from verified subject matter experts
Document Format (1 attachment)
33-E-M-S-E-M-S (244).docx