Question: A copper-silver bimetallic wire, 1 cm in diameter, is prepared by co-extrusion with copper as the core and silver as the outer layer. The desired
(a) Thermal conductivity > 410 W/(m K);
(b) Electrical conductivity > 60 Ã 106 ¦-1m-1; and
(c) Weight Determine the allowed range of the diameter of the copper core.
.png)
Copper Silver 8.96 Density (g/em3) Electrical conductivity (-1 m-1) 59x10 63x10 Thermal conductivity W( K)] 401 429 10.49
Step by Step Solution
3.37 Rating (166 Votes )
There are 3 Steps involved in it
The thermal conductivity of the composite wire k c parallel to the wire length is given by k c f Cu k cu f Ag k Ag Where f Cu and f Ag are the volume ... View full answer
Get step-by-step solutions from verified subject matter experts
Document Format (1 attachment)
814-P-M-S (1424).docx