Question: A carburizing process is carried out on a 0.10% C steel by introducing 1.0% C at the surface at 980 C, where the iron is

A carburizing process is carried out on a 0.10% C steel by introducing 1.0% C at the surface at 980 ˚C, where the iron is FCC. Calculate the carbon content at 0.01 cm, 0.05 cm, and 0.10 cm beneath the surface after 1 h?

Step by Step Solution

3.54 Rating (164 Votes )

There are 3 Steps involved in it

1 Expert Approved Answer
Step: 1 Unlock

D 023 exp 32 900 1987 12... View full answer